Michelman® Michem® Emulsion 44730 Nonionic ethylene acrylic acid copolymer

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 44730 Nonionic ethylene acrylic acid copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic ethylene acrylic acid copolymerUsage: Michem® Emulsion 44730 as a formalin and APE free additive which provides anti-slip and black heel mark resistance. These properties are quite useful in floor polish applications.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 69.5 - 70.5 %
69.5 - 70.5 %
pH 2.0 - 12
2.0 - 12
Recommended pH of system
8.7 - 9.7
8.7 - 9.7
Brookfield Viscosity <= 50 cP
<= 50 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Translucent liquid
Emulsifier Charge Nonionic
Solids Type Ethylene Acrylic Acid Copolymer