Michelman® Michem® Emulsion 41740 Nonionic, polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 41740 Nonionic, polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic, polyethylene emulsionUsage: Michem® Emulsion 41740 is used for release and water resistance in specialty coated films and papers. It is also an effective tactile modifier for interior automotive coatings. It can help give synthetic materials the draggy feel of leather.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.950 - 0.970 g/cc
0.950 - 0.970 g/cc
Volatiles 59.5 - 60.5 %
59.5 - 60.5 %
pH 1.0 - 12
1.0 - 12
Recommended pH of system
4.0 - 10
4.0 - 10
Brookfield Viscosity <= 200 cP
<= 200 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance Milky white liquid
Emulsifier Charge Nonionic
Solids Type Polyethylene