Michelman® Michem® Clean 1188 Cleaning solution

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Clean
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Clean 1188 Cleaning solution.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Cleaning solution for Indigo WS6600Usage: Michem® Clean 1188 is the recommended cleaning solution for Michem® In-Line Primer 030 priming solution. This cleaner should be added to the cleaning tank of the in-line priming unit.When manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 (Restricted)Food Contact Information when manufactured in Belgium:FDA:175.105: Components of adhesives.175.300: Resinous and polymeric components of coatings. 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
pH 8.0 - 10
8.0 - 10
Brookfield Viscosity <= 5.0 cP
<= 5.0 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Clear, colorless solution