Material Notes:
Description: Waxable white coatingUsage: MaxWhite® 17 is a white coating designed to offer excellent brightness before and after wax. This product is both hot melt and cold set gluable. Application data: MaxWhite™ 17 when applied with an 8 rod on kraft liner should provide brightness in the low to mid 80's.Typical uses include: Corrugated containers for produce; Corrugated containers for meats; Corrugated containers for citrus and Retail packagingFood Contact Information when manufactured in the USA:FDA: 176.170: Components of paper and paperboard in contact with aqueous and fatty foods(Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.65 - 1.67 g/cc
1.65 - 1.67 g/cc
pH 8.5 - 9.5
8.5 - 9.5
Brookfield Viscosity 100 - 1000 cP
100 - 1000 cP
Spindle # 3, rpm 60
Viscosity Measurement 10 - 24
10 - 24
[sec], EZ cup, Cup # 3
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance White liquid
Solids Type Polymer/Pigment