Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Hydrosize® PP2-01 Nonionic polypropylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Michelman®
Trade Name Hydrosize®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Hydrosize® PP2-01 Nonionic polypropylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic polypropylene emulsionUsage: Hydrosize® PP2-01 is an APE-free sizing for fiberglass for LFT and carbon fiber with excellent bond strength.Application data: Small particle size PP sizingInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.960 - 1.00 g/cc
0.960 - 1.00 g/cc
Volatiles 59 - 61.5 %
59 - 61.5 %
pH 8.5 - 10.5
8.5 - 10.5
Brookfield Viscosity 50 - 100 cP
50 - 100 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance Translucent, light yellow/tan liquid
Emulsifier Charge Anionic/Nonionic
Solids Type Maleated Polypropylene