Material Notes:
Description: Anionic polyamide dispersionUsage: Hydrosize® PA845 is an APE free, aqueous nylon dispersion designed to be used as a fiber sizing in fiber reinforced nylon composites where greater thermal stability is required. This small particle size dispersion has excellent film forming properties and produces high strand integrity, and is solvent and VOC free.When manufactured in USA product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 and Commission Regulation (EU) n° 10/2011(Restricted) Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.940 - 1.00 g/cc
0.940 - 1.00 g/cc
Volatiles 76 - 78 %
76 - 78 %
pH 9.7 - 10.7
9.7 - 10.7
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Alkali dispersed
Solids Type Polyamide