Material Notes:
Description: Nonionic phenoxy dispersionUsage: Hydrosize® HP3-02 is designed to be used as a fiber sizing coating with a high Tg and excellent adhesion.When manufactured in USA product meets food contact regulations for: Europe: Commission Regulation (EU) n° 10/2011(Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.06 - 1.08 g/cc
1.06 - 1.08 g/cc
Volatiles 67 - 69 %
67 - 69 %
pH 6.5 - 8.5
6.5 - 8.5
Brookfield Viscosity <= 4000 cP
<= 4000 cP
Spindle # 4, rpm 60
Descriptive Properties Value Comments
Appearance Milk white
Emulsifier Charge Nonionic
Solids Type Phenoxy Dispersion