Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® DigiPrime® 4431 Primer

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name DigiPrime®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® DigiPrime® 4431 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Primer for digital printingUsage: DigiPrime® 4431 is a patented flexo and gravure ready coating which provides excellent adhesion of HP Indigo ElectroInks® to a variety of films. This product is suitable for food contact and so is especially useful for flexible packaging applications as well as label production.Application data: DigiPrime® 4431 may be applied by flexo, gravure, rod or roll coating systems.Food Contact Information when manufactured in Belgium, Singapore and USA:FDA: 175.105: Components of adhesives 175.300: Resinous and polymeric components of coatings.(Restricted)175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)When manufactured in Belgium, Singapore and USA product meets food contact regulations for: Europe: Euro. Res. AP(2004)1(Restricted) and Commission Regulation (EU) n° 10/2011(Restricted)Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 71 - 72.5 %
71 - 72.5 %
pH 8.0 - 10
8.0 - 10
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance White, translucent liquid
Users viewing this material also viewed the following: