Michelman® DigiPrime® 2000 Primer

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name DigiPrime®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® DigiPrime® 2000 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Primer for digital printing Usage: DigiPrime® 2000 is flexo and gravure ready and provides excellent adhesion of Indigo inks to uncoated, mottled, semi-gloss and glossy paper grades. This product also improves the rub resistance of Indigo inks and does not yellow with time.Application data: DigiPrime ® 2000 may be applied by flexo, gravure, rod or roll coating systemsFood Contact Information when manufactured in the USA and Belgium:FDA: 175.105: Components of adhesives175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)176.180: Components of paper and paperboard in contact with dry foods.When manufactured in USA product meets food contact regulations for: Europe: Euro. Res. AP(2004)1Germany:BfR Recommendation When manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1(Restricted) Germany:BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 74 - 76 %
74 - 76 %
pH 7.8 - 8.8
7.8 - 8.8
Brookfield Viscosity <= 60 cP
<= 60 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance White liquid