MetalTek WC 6 Cast UNS J24054 Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel , AISI 4000 Series Steel
Manufacturer MetalTek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek WC 6 Cast UNS J24054 Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 285
285
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
Tensile Strength, Yield >= 275 MPa
>= 39900 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Carbon, C 0.05 - 0.20 %
0.05 - 0.20 %
Chromium, Cr 1.0 - 1.5 %
1.0 - 1.5 %
Iron, Fe 96.25 - 98 %
96.25 - 98 %
As Balance
Manganese, Mn 0.50 - 0.80 %
0.50 - 0.80 %
Molybdenum, Mo 0.45 - 0.65 %
0.45 - 0.65 %
Silicon, Si <= 0.60 %
<= 0.60 %
Descriptive Properties Value Comments
Heat Treatment Quench & Temper