MetalTek MTEK HC-225 UNS F45005 Abrasion Resistant Cast Iron

Category Metal , Ferrous Metal , Cast Iron , Superalloy , Iron Base
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK HC-225 UNS F45005 Abrasion Resistant Cast Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Restrict to low stress applications. Resists oxidation and high sulfur flue gas.Applications: Tuyeres, gas dampers, salt pots, support skids.Information provided by MetalTek
Component Elements Properties Metric English Comments
Carbon, C 2.0 - 3.3 %
2.0 - 3.3 %
Chromium, Cr 14 - 18 %
14 - 18 %
Iron, Fe 69.7 - 84 %
69.7 - 84 %
As Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo <= 3.0 %
<= 3.0 %
Nickel, Ni <= 2.5 %
<= 2.5 %
Silicon, Si <= 1.5 %
<= 1.5 %