MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High aqueous and atmospheric corrosion resistance, moderate strength and conductivity.Applications: Valves, pumps, pipe fittings, electric terminal ends.Information provided by MetalTekCast UNS C83600; Cast Grade C83600; Cast ASTM B271, B62, B584; Military MIL-C-15345-14; SAE 40 (Discontinued)
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
500 kg
Tensile Strength, Ultimate >= 205 MPa
>= 29700 psi
Tensile Strength, Yield >= 95.0 MPa
>= 13800 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Copper, Cu 85 %
85 %
Lead, Pb 5.0 %
5.0 %
Tin, Sn 5.0 %
5.0 %
Zinc, Zn 5.0 %