MetalTek MTEK 825 Cast UNS N08826 Severe Corrosion and Heat Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 825 Cast UNS N08826 Severe Corrosion and Heat Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 515 MPa
>= 74700 psi
Tensile Strength, Yield >= 340 MPa
>= 49300 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 19.5 - 23.5 %
19.5 - 23.5 %
Copper, Cu 1.5 - 3.5 %
1.5 - 3.5 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 2.5 - 3.5 %
2.5 - 3.5 %
Nickel, Ni 38 - 44 %
38 - 44 %
Niobium, Nb (Columbium, Cb) 0.60 - 1.2 %
0.60 - 1.2 %
Silicon, Si <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal