MetalTek MTEK 79-6-15 HI LEAD Cast UNS C93900 Bearing Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 79-6-15 HI LEAD Cast UNS C93900 Bearing Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Popular alloy with score resistance, structural uniformity, shear properties, compressive strength and low cost.Applications: Bearings, bushings, sleeves, liners, piston rings, hydraulic partsInformation provided by MetalTekCast UNS C93900; Cast Grade C93900; Cast ASTM B66; Mil QQ-C-390B
Mechanical Properties Metric English Comments
Hardness, Brinell 60
60
500 kg
Tensile Strength, Ultimate >= 170 MPa
>= 24700 psi
Tensile Strength, Yield >= 110 MPa
>= 16000 psi
Elongation at Break >= 5.0 %
>= 5.0 %
Component Elements Properties Metric English Comments
Copper, Cu 79 %
79 %
Lead, Pb 15 %
15 %
Tin, Sn 6.0 %
6.0 %