MetalTek MTEK 29-4 Cast UNS J92605 Heat Resistant Stainless Steel

Category Metal , Ferrous Metal , Heat Resisting , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 29-4 Cast UNS J92605 Heat Resistant Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Restrict to low stress applications. Resists oxidation and high sulfur flue gas.Applications: Tuyeres, gas dampers, salt pots, support skids.Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 380 MPa
>= 55100 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 650 °C
1200 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.50 %
<= 0.50 %
Chromium, Cr 26 - 30 %
26 - 30 %
Iron, Fe 62.5 - 74 %
62.5 - 74 %
As Balance
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni <= 4.0 %
<= 4.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated