MetalTek MTEK 25-35 Cast UNS N08705; Cast UNS J95705 Heat Resistant Stainless Steel

Category Metal , Ferrous Metal , Heat Resisting , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 25-35 Cast UNS N08705; Cast UNS J95705 Heat Resistant Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Higher chrome and nickel content provides increased strength and resistance to both oxidation and carburization.Applications: Reformer and Ethylene pyrolysis tubes and fittings.Information provided by MetalTekCast UNS N08705; J95705; Cast Grade HP; Cast ASTM A297
Mechanical Properties Metric English Comments
Hardness, Brinell 190
190
Tensile Strength, Ultimate >= 430 MPa
>= 62400 psi
Tensile Strength, Yield >= 235 MPa
>= 34100 psi
Elongation at Break >= 4.5 %
>= 4.5 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1050 °C
1920 °F
Component Elements Properties Metric English Comments
Carbon, C 0.35 - 0.75 %
0.35 - 0.75 %
Chromium, Cr 24 - 28 %
24 - 28 %
Iron, Fe 29.75 - 42.65 %
29.75 - 42.65 %
As Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 33 - 37 %
33 - 37 %
Silicon, Si <= 2.5 %
<= 2.5 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated