MetalTek ESCOLOY 45D® Cast UNS J93345 Duplex Stainless Steel

Category Metal , Ferrous Metal , Duplex , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name ESCOLOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek ESCOLOY 45D® Cast UNS J93345 Duplex Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels. Produced under license of ESCO Corp.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, valve trim, pulp digesters Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 217
217
Tensile Strength, Ultimate >= 655 MPa
>= 95000 psi
Tensile Strength, Yield >= 450 MPa
>= 65300 psi
Elongation at Break >= 25 %
>= 25 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 22.5 - 25.5 %
22.5 - 25.5 %
Iron, Fe 55.62 - 66.4 %
55.62 - 66.4 %
As Balance
Manganese, Mn <= 1.5 %
<= 1.5 %
Molybdenum, Mo 3.0 - 4.5 %
3.0 - 4.5 %
Nickel, Ni 8.0 - 11 %
8.0 - 11 %
Nitrogen, N 0.10 - 0.30 %
0.10 - 0.30 %
Silicon, Si <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal