MetalTek Copper Ni Si Cast UNS C81540 High Conductivity

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer MetalTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek Copper Ni Si Cast UNS C81540 High Conductivity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTekCast Grade C81540
Mechanical Properties Metric English Comments
Hardness, Brinell 192
192
3000 kg, typical
Tensile Strength, Ultimate >= 550 MPa
>= 79800 psi
Tensile Strength, Yield >= 450 MPa
>= 65300 psi
Elongation at Break >= 15 %
>= 15 %
Component Elements Properties Metric English Comments
Chromium, Cr 0.10 - 0.60 %
0.10 - 0.60 %
Copper, Cu 95.6 - 97.5 %
95.6 - 97.5 %
Nickel, Ni 2.0 - 3.0 %
2.0 - 3.0 %
Silicon, Si 0.40 - 0.80 %
0.40 - 0.80 %