MetalTek C86500 Low Tensile Manganese Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek C86500 Low Tensile Manganese Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High aqueous and atmospheric corrosion resistance, moderate strength and conductivity.Applications: Valves, pumps, pipe fittings, electric terminal ends.Information provided by MetalTekCast UNS C83650; Cast Grade C83650; Cast ASTM B271, B584, B148; Military MIL-C-15345-4; SAE 43 (Discontinued)
Mechanical Properties Metric English Comments
Hardness, Brinell 149
149
Tensile Strength, Ultimate >= 450 MPa
>= 65300 psi
Tensile Strength, Yield >= 170 MPa
>= 24700 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Aluminum, Al 1.0 %
1.0 %
Copper, Cu 58 %
58 %
Iron, Fe 1.0 %
1.0 %
Manganese, Mn 1.0 %
1.0 %
Zinc, Zn 39 %
39 %