MetalTek C11600 Silver Copper High Conductivity

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer MetalTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek C11600 Silver Copper High Conductivity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical property data from forged samples.Information provided by MetalTekCast UNS C11600; Cast Grade C11600
Mechanical Properties Metric English Comments
Hardness, Brinell 79
79
500 kg
Tensile Strength, Ultimate >= 235 MPa
>= 34100 psi
Tensile Strength, Yield >= 205 MPa
>= 29700 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Copper, Cu >= 99.9 %
>= 99.9 %
Silver, Ag >= 0.085 %
>= 0.085 %