Meilian Chemical PE650 GREEN MASTERBATCH

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Meilian Chemical Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meilian Chemical PE650 GREEN MASTERBATCH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GREEN PE650 is a green LDPE based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Green 7.Method of Usage: GREEN PE 650 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, avoiding pollution and malscattering problems caused by pigment.Range of Application: GREEN PE650 is designed for use in LDPE, HDPE, LLDPE and PP for production of premium high glossy films.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
High Load Melt Index 18 g/10 min

@Load 21.6 kg,
Temperature 190 °C
18 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content 30