Material Notes:
Type HE is a freely machinable material in the as-cast condition. Withstands rapid heating and cooling without premature failure, offers good dimensional stability and a good range of strength properties. Recommended for ingot molds, slag pots, hot plates, and parts heated rapidly by a naked flame.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Mechanical Properties Metric English Comments
Hardness, Brinell 170
170
Nominal
Tensile Strength, Ultimate 172 MPa
25000 psi
Modulus of Elasticity 68.9 GPa
10000 ksi
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 37.8 - 538 °C
6.66 µin/in-°F

@Temperature 100 - 1000 °F
Thermal Conductivity 42.9 W/m-K

@Temperature 10.0 - 232 °C
298 BTU-in/hr-ft²-°F

@Temperature 50.0 - 450 °F