Material Notes:
Type WSH is an austenitic nodular iron possessing superior tensile strength, toughness and ability to work harden under conditions of severe pounding impact. It is extremely difficult to machine. Recommended for crusher liners, hammers, grinding balls, etc.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Mechanical Properties Metric English Comments
Hardness, Brinell 350 - 500
350 - 500
Nominal
Tensile Strength, Ultimate 689 MPa
100000 psi
Tensile Strength, Yield 517 MPa
75000 psi
Elongation at Break 4.0 - 10 %
4.0 - 10 %
Modulus of Elasticity 165 GPa
24000 ksi
Izod Impact Unnotched <= 163 J

@Diameter 30.5 mm
<= 120 ft-lb

@Diameter 1.20 in
bar