Meehanite Almanite® W4 Wear and Abrasion Resisting Cast Iron

Category Metal , Ferrous Metal , Austenitic , Cast Iron , White Cast Iron , Martensitic
Manufacturer Meehanite
Trade Name Almanite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meehanite Almanite® W4 Wear and Abrasion Resisting Cast Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type W4 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W4 is highly alloyed to provide an austenitic matrix in the as-cast condition which may be further modified to give martensitic matrix by heat treatment or by freezing. General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Mechanical Properties Metric English Comments
Hardness, Brinell 400 - 700
400 - 700
Nominal
Tensile Strength, Ultimate 414 - 552 MPa
60000 - 80000 psi
Izod Impact Unnotched 54.2 - 94.9 J

@Diameter 30.5 mm
40.0 - 70.0 ft-lb

@Diameter 1.20 in
bar