McDanel Advanced Ceramics MV-30 Mullite

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer McDanel Advanced Ceramics, Ltd
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF McDanel Advanced Ceramics MV-30 Mullite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by McDanel Advanced Ceramic Technologies
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength 180 MPa
26100 psi
Compressive Strength 1310 MPa
190000 psi
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 1000 °C
3.00 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 6.00 W/m-K
41.6 BTU-in/hr-ft²-°F
3.60 W/m-K

@Temperature 800 °C
25.0 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1680 °C
3060 °F
no load
Component Elements Properties Metric English Comments
Al2O3 60 %
60 %
CaO 0.10 %
0.10 %
Fe2O3 0.50 %
0.50 %
K2O 0.60 %
0.60 %
MgO 0.20 %
0.20 %
Na2O 0.20 %
0.20 %
SiO2 37.9 %
37.9 %
TiO2 0.50 %
0.50 %