Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Matrixx Group 84S7301 Flame Retardant 30% Glass Reinforced PET (V0)  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Matrixx Group 84S7301 Flame Retardant 30% Glass Reinforced PET (V0)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by The Matrixx Group, formerly RePlas.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
73°F; ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 131 MPa
19000 psi
0.125 in; ASTM D638
Flexural Modulus 9.31 GPa
1350 ksi
Tangent, 0.125 in; ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0.125 in, 73°F; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Relative Thermal Index; UL746
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
0.125 in; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
395 °F
0.125 in; ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Users viewing this material also viewed the following: