Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name MoldMAX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12” and in rounds up to 23.5”, moldMAX XL® can be used as a direct replacement for P-20 tool steels. moldMAX XL® provides an exciting combination of strength and thermal conductivity – the strength of prehardened tool steels and the high conductivity of copper – in larger cross sections for bigger molds. For large tools, this combination provides unbeatable economic value for the molder, and the excellent machinability means metal removal rates are high as well. Machines 5 times faster than P-20 steel. The high strength and hardness ensures that moldMAX XL® tools will provide durability as well as efficiency.Information supplied by Brush Wellman Engineered Materials.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28 - 32
28 - 32
Tensile Strength, Ultimate 758 MPa
110000 psi
Tensile Strength, Yield 689 MPa

@Strain 0.200 %
100000 psi

@Strain 0.200 %
Elongation at Break 4 %
4 %
in 2"
Modulus of Elasticity 117 GPa
17000 ksi
Charpy Impact 13.6 - 20.3 J
10.0 - 15.0 ft-lb
V-Notch
Thermal Properties Metric English Comments
CTE, linear 16.7 µm/m-°C

@Temperature 20.0 °C
9.30 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.381 J/g-°C
0.0910 BTU/lb-°F
Thermal Conductivity 60.5 - 69.2 W/m-K
420 - 480 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 316 °C
600 °F
Continuous
Component Elements Properties Metric English Comments
Copper, Cu 90 %
90 %
Nickel, Ni 9.0 %
9.0 %
Tin, Sn 1.0 %
1.0 %
Users viewing this material also viewed the following: