Master Bond UV15X-2 One Component, Non-Yellowing UV Curable Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond UV15X-2 One Component, Non-Yellowing UV Curable Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond UV15X-2 is a one component, non-yellowing UV curable polymer system for high performance coatings, adhesives and sealants with exceptionally fast response to UV radiation. The cured coatings, adhesives and sealants can be used over the exceptionally wide temperature range of -60°F to +300°F.
Physical Properties Metric English Comments
Viscosity 6000 - 8000 cP

@Temperature 23.0 °C
6000 - 8000 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Descriptive Properties Value Comments
Color Transparent