Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond UV15DC80 is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curing areas on parts that do not allow UV light curing because of “shadowing” issues. Most noteworthy is that the heat cure portion can be initiated at only 80°C rather than at the more common 125°C.
Physical Properties Metric English Comments
Viscosity 50000 - 70000 cP
50000 - 70000 cP
uncured coating
Mechanical Properties Metric English Comments
Hardness, Shore D >= 70
>= 70
Tensile Strength >= 34.5 MPa
>= 5000 psi
Tensile Modulus >= 2.41 GPa
>= 350 ksi
Thermal Properties Metric English Comments
CTE, linear 55.0 - 65.0 µm/m-°C
30.6 - 36.1 µin/in-°F
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Glass Transition Temp, Tg >= 125 °C
>= 257 °F
with post cure
Optical Properties Metric English Comments
Refractive Index 1.52
1.52
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.49

@Frequency 60.0 Hz
3.49

@Frequency 60.0 Hz
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
in original unopened containers
Descriptive Properties Value Comments
Chemical Resistance Water
<1% weight gain, 30 month immersion, 75°F