Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name Supreme
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applications where long term exposure to temperatures from -78°to +450°F (-55°to+228°C) is required. It is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly at elevated temperatures with a 100 to 30 mix ratio, by weight, to produce high bonding strengths at both ambient and elevated temperatures which unlike that of many other epoxy adhesives, are relatively insensitive to small changes in the mix ratio or substrate cleaning procedures. Master Bond Polymer Adhesive SUPREME 45HTND can be applied without sagging or dripping on vertical surfaces. It produces durable high strength and tough bonds which are resistant to thermal cycling and chemicals including water, oil and most organic solvents over the wide temperature range of -80°F to more than +450°F. Adhesion to metals, glass, ceramics, wood, vulcanized rubber and many plastics is excellent. The hardened adhesive is an electrical insulator, Color of Part A is gray, part B is clear brown. Master Bond Polymer Adhesive SUPREME 45HTND is widely used in aerospace, electronic, electrical, computer, construction, metal working, appliance, automotive and chemical industries. Product Advantages: Convenient mixing: product properties relatively unaffected by small changes in mix ratio Surface cleanliness not critical for good bonding in many uses but needed for optimal strength Easy application contact pressure only required for cure, adhesive spreads evenly and smoothly; no drip application feature Convenient cure schedules: long pot life at room temperature and fast elevated temperature cures as requiredHigh bonding strength to similar and dissimilar substrates with superior peel strengthSuperior durability, thermal shock and chemical resistance 100% reactive and does not contain any solvents or diluentsResists ET0 sterilizationInformation provided by MasterBond®
Mechanical Properties Metric English Comments
Shear Strength >= 15.9 MPa
>= 2300 psi
Bond, Al to Al, after 30 days water immersion
>= 17.2 MPa
>= 2500 psi
Bond, Al to Al
Peel Strength >= 2.10 kN/m
>= 12.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 135 - 163 °C
2.00 - 3.00 hour

@Temperature 275 - 325 °F
Pot Life >= 720 min
>= 720 min
200 gram mass
>= 720 min
>= 720 min
1 quart mass
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Mixing Ratio (A to B) 100/30
by weight