Master Bond Mastersil 803 One component Room Temperature Curing Non- Corrosive Silicone

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Mastersil 803 One component Room Temperature Curing Non- Corrosive Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond MasterSil 803 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This material is a clear non-corrosive flowable compound which can be easily handled and processes readily.
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 4.48 MPa
650 psi
Elongation at Yield 300 %
300 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -118 °C
-180 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Processing Properties Metric English Comments
Cure Time 4320 - 5760 min

@Temperature 23.0 °C
72.0 - 96.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Translucent
Set-Up Time, minutes 30-40
At Room Temperature
Viscosity Paste