Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond Mastersil 726 Conductive Silicone Compound for Heat Transfer

Category Fluid , Lubricant , Silicone Base , Silicone, Filled Grease
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Mastersil 726 Conductive Silicone Compound for Heat Transfer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System MasterSil 726 is a non-curing grease-like thermally conductive silicone compound. It is extremely stable, it will not dry out, cure, harden, or bleed, even after exposure to temperatures as high as 200C (392F).
Thermal Properties Metric English Comments
Thermal Conductivity 0.720 - 0.865 W/m-K
5.00 - 6.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Descriptive Properties Value Comments
Color Opaque White
Viscosity Paste