Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive

Category Polymer , Thermoset , Silicone
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of 0.75 mm and 1.5 mm, and 94V-0 for a 3 mm thickness. It adheres well to a wide variety of substrates including glass, metals and many plastics. The rapidity of the cure depends on the thickness of the layer and the humidity; the thicker the layer the slower the cure. It is soft with good elasticity and flexibility, and outstanding electrical insulation properties. Most importantly, it is non-corrosive, fast setting, and has a paste like consistency. MasterSil 707FR is serviceable over the broad temperature range of -45°C to +200°C, as per UL specifications, and is gray in color. Key Features UL listed for 94V-1 and 94V-0 Very fast cure Non-corrosive Good adhesion propertiesInformation provided by MasterBond®
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 45
35 - 45
Tensile Strength at Break 2.76 - 3.45 MPa
400 - 500 psi
Elongation at Break 300 - 400 %
300 - 400 %
Shear Strength 1.03 - 1.38 MPa
150 - 200 psi
Tensile, Al to Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.2

@Frequency 60.0 Hz,
Temperature 25.0 °C
3.2

@Frequency 60.0 Hz,
Temperature 77.0 °F
Dielectric Strength 23.6 kV/mm

@Thickness 3.17 mm
600 kV/in

@Thickness 0.125 in
Dissipation Factor 0.010

@Frequency 60.0 Hz,
Temperature 25.0 °C
0.010

@Frequency 60.0 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 - 10.0 min
0.0833 - 0.167 hour
Tack-free time
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Descriptive Properties Value Comments
Appearance gray