Material Notes:
Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In fact, this system will fully cure tack-free without any oxygen inhibition. This breakthrough technology allows LED401 to be utilized not only as an adhesive, but as a sealant, coating and encapsulation material. This system can cure in sections up to and beyond 1/8 inch thick upon exposure to the LED light. Since it is a LED curable system, it is intrinsically safer than one requiring UV light for polymerization, as LED light emitting sources are generally considered to be less hazardous and more user friendly than their comparable UV counterparts.
Physical Properties Metric English Comments
Viscosity 100000 - 150000 cP
100000 - 150000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
Tensile Strength >= 24.1 MPa
>= 3500 psi
Tensile Modulus 0.276 - 0.552 GPa
40.0 - 80.0 ksi
Thermal Properties Metric English Comments
CTE, linear 60.0 - 65.0 µm/m-°C
33.3 - 36.1 µin/in-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Glass Transition Temp, Tg 70.0 - 75.0 °C
158 - 167 °F
Optical Properties Metric English Comments
Transmission, Visible >= 90 %
>= 90 %
thickness not specified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.7

@Frequency 60.0 Hz
3.7

@Frequency 60.0 Hz
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
unopened containers with no exposure to light
Descriptive Properties Value Comments
Color Clear