Material Notes:
Description: Master Bond Polymer System EP42HT-2AN is a room temperature curable two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance and outstanding chemical resistance. It is widely used, particularly in medical products, because it is capable of withstanding repeat sterilization including radiation, ethylene oxide, chemical sterilants, and steam sterilization. In addition, it fully complies with the testing requirements for USP Class VI plastics. Aside from being a superior adhesive, sealant and coating, EP42HT-2AN is castable to thicknesses exceeding 3-4 inches. EP42HT-2AN cures readily at ambient temperatures or more quickly at elevated temperatures even in the presence of moisture. The cured epoxy compound is resistant not only to various types of sterilization, but also to inorganic and organic acids, alkalis, many organic solvents, aromatic hydrocarbons, etc. EP42HT-2AN is an excellent electrical insulator. Especially noteworthy is its serviceability from -100F up to 400°F combined with being relatively impervious to intermittent exposures to steam. Aside from its widespread use in the medical industry, EP42HT-2AN is also used in electronics, electrical, fiberoptic and optical as well as OEM type applications. Product Advantages: Convenient non-critical 100:40 mix ratio by weight. Contains no solvents. Convenient cure schedules at both ambient and elevated temperatures. Outstanding resistance to medical sterilants including radiation, ETO, chemicals and steam. Excellent chemical resistance to acids, alkalis and many solvents. Superior thermal stability; serviceable from -100°F up to 400°F. Castable to thicknesses exceeding 3-4 inches. Outstanding thermal conductivity.Information provided by MasterBond®
Physical Properties Metric English Comments
Viscosity 4000 cP
4000 cP
Part B
325000 cP
325000 cP
Part A
Mechanical Properties Metric English Comments
Hardness, Shore D >= 80
>= 80
Elongation at Break >= 2.0 %
>= 2.0 %
Shear Strength >= 6.89 MPa
>= 1000 psi
Tensile lap, Al to Al
Thermal Properties Metric English Comments
CTE, linear 30.0 - 35.0 µm/m-°C
16.7 - 19.4 µin/in-°F
Thermal Conductivity 3.17 - 3.60 W/m-K
22.0 - 25.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
2880 - 4320 min

@Temperature 23.9 °C
48.0 - 72.0 hour

@Temperature 75.0 °F
Pot Life 60 - 75 min
60 - 75 min
100 gram batch
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in unopened container
Descriptive Properties Value Comments
Mixing Ratio (A to B) 100/40
by weight