Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP37-3 Optically Clear, Impact Resistant Two Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP37-3 Optically Clear, Impact Resistant Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP37-3 is a low viscosity, resilient, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. As an adhesive, it forms tough high strength bonds that offer excellent impact resistance as well as resistance to thermal cycling. It bonds well to a wide variety of substrates including metals, glass, ceramics, rubber and many plastics.
Physical Properties Metric English Comments
Viscosity 300 - 400 cP

@Temperature 23.0 °C
300 - 400 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 240 - 360 min

@Temperature 93.3 °C
4.00 - 6.00 hour

@Temperature 200 °F
7200 - 10100 min

@Temperature 23.0 °C
120 - 168 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Clear; "B" Clear
Mix Ratio By Weight 100/50
Set-Up Time, minutes min 360
At Room Temperature