Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapidly at elevated temperatures. It has a ten to one (10:1) mix ratio by weight. EP30AOHT has an attractive balance of performance properties including high thermal conductivity, excellent electrical insulation characteristics and dimensional stability, as well as a good physical strength profile. The system has excellent flow properties making it ideal as a thermally conductive, electrically insulating potting epoxy. EP30AOHT is also an adhesive/sealant forming durable rigid bonds that are resistant to thermal cycling and chemicals including water, oil and most solvents, over the wide temperature range of -60°F to +400°F. The thermal expansion coefficient is exceptionally low: 22-25 ppm/°C. Color of Part A is of f white, Part B is clear. Master Bond EP30AOHT is widely used in the electronic, electrical, computer and chemical industries where electrical insulation and environmental protection are required and heat transfer must be maintained. Product Advantages: Easy application: adhesive spreads or pours evenly and smoothly. Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required. High bond strength to a wide variety of substrates; excellent adhesive properties. High thermal conductivity with exceptional electrical insulation properties. Low thermal expansion coefficient; superior dimensional stability. Good physical strength characteristics; especially high compressive strength. Excellent flowability; suitable for potting and casting. High temperature resistance; serviceable to 400°F.Information provided by MasterBond®
Physical Properties Metric English Comments
Viscosity 280 - 500 cP
280 - 500 cP
Part B
380000 - 430000 cP
380000 - 430000 cP
Part A
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Tensile Strength at Break >= 51.7 MPa
>= 7500 psi
Compressive Strength >= 138 MPa
>= 20000 psi
Shear Strength >= 8.27 MPa
>= 1200 psi
Tensile, Al to Al
Thermal Properties Metric English Comments
CTE, linear 22.0 - 25.0 µm/m-°C
12.2 - 13.9 µin/in-°F
Thermal Conductivity 1.30 - 1.44 W/m-K
9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
4.0

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
4.3

@Frequency 1000 Hz,
Temperature 25.0 °C
4.3

@Frequency 1000 Hz,
Temperature 77.0 °F
4.5

@Frequency 60.0 Hz,
Temperature 25.0 °C
4.5

@Frequency 60.0 Hz,
Temperature 77.0 °F
Dielectric Strength >= 15.7 kV/mm

@Thickness 3.17 mm
>= 400 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 93.3 °C
1.00 - 2.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Pot Life 30 - 45 min
30 - 45 min
100 gram batch
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened container
Descriptive Properties Value Comments
Mixing Ratio (A to B) 10:1
by weight
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved