Material Notes:
Description: Master Bond Polymer System EP30-D10 is a versatile two component, abrasion resistant elastomer featuring superior strength, toughness and chemical resistance for high performance bonding, sealing, casting and encapsulation. It combines the performance characteristics of epoxy resins such as strength, chemical resistance, and adhesive qualities, with those of the polyurethanes including toughness, abrasion resistance and flexibility. In addition, EP30D10 has been used successfully in a number of different cryogenic applications. Master Bond Polymer System EP30D-10 is formulated to cure at room temperature or more rapidly at elevated temperatures. Master Bond Polymer System EP30D-10 is 100% reactive and does not contain any solvents or diluents. The Master Bond EP30D-10 system cures with minimal shrinkage to a durable, high strength, tough elastomer with good resistance to thermal cycling and chemicals including water, inorganic salts, alkalis and acids. It has an wide service temperature range of 4K to 220°F. Adhesion to metals, concrete, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. Color of part A is clear, part B is also clear. Master Bond Polymer System EP30D-10 is widely used in cryogenic, optical, electronic and aerospace applications both for original components and maintenance/repair. A non-drip version (amber colored) called EP30D-10ND is also available. Product Advantages: Long working life. Versatile cure schedules; ambient temperature cures or fast cures at elevated temperatures as required. High bonding strength to similar and dissimilar substrates including metals, rubbers, ceramics. High impact strength, fatigue resistance and flexibility. Low water absorption, low moisture permeability. Superior retention of mechanical, chemical properties upon thermal cycling. Excellent electrical insulation properties. Temperature range,4K to 220°F; cryogenically serviceable. 100% solids formulation; no solvents or diluents; minimal shrinkage upon curing. Excellent optical properties; superior non-yellowing.Information provided by MasterBond®
Physical Properties Metric English Comments
Viscosity >= 100000 cP
>= 100000 cP
mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break >= 10.3 MPa
>= 1500 psi
Elongation at Break >= 150 %
>= 150 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 104 °C
220 °F
Minimum Service Temperature, Air -168 °C
-270 °F
Processing Properties Metric English Comments
Cure Time 240 - 300 min

@Temperature 93.3 °C
4.00 - 5.00 hour

@Temperature 200 °F
4320 - 7200 min

@Temperature 23.9 °C
72.0 - 120 hour

@Temperature 75.0 °F
Pot Life 180 min
180 min
100 gram batch
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
in unopened container
Descriptive Properties Value Comments
Appearance transparent
Mixing Ratio (A to B) 100/05
weight basis