Master Bond EP27 Low Temperature Curing Two Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP27 Low Temperature Curing Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP27 is a unique two component epoxy formulation offers relatively fast cures at temperatures as low as 40°F and below, with curing times much shorter than currently existing products. Also EP27 feature remarkably high physical strength properties, superior chemical resistance and outstanding electrical insulation characteristics over a wide temperature range.
Physical Properties Metric English Comments
Viscosity 2100 - 2500 cP

@Temperature 23.0 °C
2100 - 2500 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 93.3 °C
1.00 - 2.00 hour

@Temperature 200 °F
720 - 1440 min

@Temperature 23.0 °C
12.0 - 24.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Clear; "B" Amber
Mix Ratio By Weight 100/50
Set-Up Time, minutes 25-30
At Room Temperature