Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP22 Aluminum Filled Tough Two Component Epoxy Compound

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP22 Aluminum Filled Tough Two Component Epoxy Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP22 is an aluminum filled, two component epoxy adhesive for high performance bonding, sealing, and coating. It is formulated to cure at room temperature or more rapidly at elevated temperatures, with a non-critical one-to-one mix ratio by weight or volume. The EP22 compound readily develops a high bond strength of 3000 psi at room temperature which unlike that of many other epoxy compositions, is relatively insensitive to mixing ratio.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
600 min

@Temperature 23.0 °C
10.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Gray; "B" Gray
Mix Ratio By Weight 100/100
Set-Up Time, minutes 60-90
At Room Temperature
Viscosity Paste
Room Temperature
Copyright © lookpolymers.com All Rights Reserved