Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP21TDCSMed Two Component, Silver Conductive USP Class VI Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP21TDCS MED is a two component, silver filled, electrically conductive adhesive/sealant that meets USP Class VI specifications for medical applications. The high strength bonds are remarkably adaptable to thermal cycling and resistant to chemicals including water, oil and most organic solvents, over the exceptionally wide temperature range of 4°K to +275 °F enabling it to be serviceable even in cryogenic applications.
Mechanical Properties Metric English Comments
Elongation at Break >= 5.0 %
>= 5.0 %
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
shear, Al/Al, after 30 days water immersion
>= 5.86 MPa
>= 850 psi
shear, Al/Al
Thermal Properties Metric English Comments
Thermal Conductivity 3.75 W/m-K
26.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -269 °C
-452 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0010 ohm-cm
<= 0.0010 ohm-cm
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 93.3 °C
1.00 - 2.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Pot Life 30 - 40 min
30 - 40 min
50 gram mass
Shelf Life 3.00 - 6.00 Month
3.00 - 6.00 Month
Descriptive Properties Value Comments
Mixing Ratio (A to B) 1/1
Viscosity smooth paste