Master Bond EP21BAS Radiopaque Two Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP21BAS Radiopaque Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP21BAS is a radiopaque epoxy compound which offers outstanding performance and superior processability. Radiopaque epoxy polymer compounds are employed for medical diagnostic and therapeutic devices to achieve optical visibility when exposed to x-rays, fluoroscopes or x-ray imaging procedures. The degree of radiopacity achieved depends on the type and amount of the filler employed, the energy capacity of the x-ray machine and the requirements of the specific medical procedure to be used.
Physical Properties Metric English Comments
Viscosity >= 175000 cP

@Temperature 23.0 °C
>= 175000 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
2880 - 3600 min

@Temperature 23.0 °C
48.0 - 60.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Off White; "B" Off White
Mix Ratio By Weight 100/100
Set-Up Time, minutes 60-90
At Room Temperature