Master Bond EP15 High Tensile Strength One Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP15 High Tensile Strength One Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP15 is a one component, heat curing epoxy featuring high tensile strength utilized in testing the adhesion and/or cohesive strength of flame-sprayed coatings. This standard test is fully detailed in ASTM specification C633. Upon cure, EP15 has a tensile strength well in excess of 12,000 psi.
Physical Properties Metric English Comments
Viscosity 90000 - 100000 cP

@Temperature 23.0 °C
90000 - 100000 cP

@Temperature 73.4 °F
Storage Temperature 23.9 °C
75.0 °F
3 months, minimum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 90.0 min

@Temperature 149 - 177 °C
1.00 - 1.50 hour

@Temperature 300 - 350 °F
Descriptive Properties Value Comments
Color Tan