MarkeTech Strontium Lanthanum Galate (SrLaGaO3) Single Crystal Substrate

Category Ceramic , Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Strontium Lanthanum Galate (SrLaGaO3) Single Crystal Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
Physical Properties Metric English Comments
a Lattice Constant 3.84 Ã…
3.84 Ã…
c Lattice Constant 12.68 Ã…
12.68 Ã…
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 °C
3.33 µin/in-°F

@Temperature 68.0 °F
Melting Point 1238 °C
2260 °F
Electrical Properties Metric English Comments
Dielectric Constant 300
300