MarkeTech Spinel (MgAl2O4) Single Crystal Substrate

Category Ceramic , Oxide , Aluminum Oxide , Magnesium Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Spinel (MgAl2O4) Single Crystal Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 9%.
Physical Properties Metric English Comments
Density 3.60 g/cc
0.130 lb/in³
a Lattice Constant 8.803 Ã…
8.803 Ã…
Thermal Properties Metric English Comments
CTE, linear 7.45 µm/m-°C

@Temperature 20.0 °C
4.14 µin/in-°F

@Temperature 68.0 °F
Melting Point 2130 °C
3870 °F
Descriptive Properties Value Comments
Crystal Structure Cubic
Users viewing this material also viewed the following: