Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MarkeTech Repton 827 Zirconia + 3 mol% Yttria (YSZ)

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Repton 827 Zirconia + 3 mol% Yttria (YSZ).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Brand 827 features: Co-precipitation high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Bulk Density 4.10 g/cc
0.148 lb/in³
Density 5.86 g/cc
0.212 lb/in³
calculated from bulk density after subtracting pore volume
Porosity 30 %
30 %
Mechanical Properties Metric English Comments
Flexural Strength >= 96.0 MPa
>= 13900 psi
Component Elements Properties Metric English Comments
Y2O3 3.0 %
3.0 %
ZrO2 97 %
97 %