MarkeTech Repton 136 Aluminum Oxide

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Repton 136 Aluminum Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Brand 136 features: Molding-structural.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Density 3.90 g/cc
0.141 lb/in³
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Flexural Strength >= 392 MPa
>= 56900 psi
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 300 °C
3.33 µin/in-°F

@Temperature 572 °F
8.00 µm/m-°C

@Temperature 900 °C
4.44 µin/in-°F

@Temperature 1650 °F
Component Elements Properties Metric English Comments
Al2O3 99.6 %
99.6 %
Descriptive Properties Value Comments
Spall Resist 550°C