MarkeTech Gallium Phosphide Semiconductor Wafer, n-type, Sulfur + Tellurium Doped, Czochralski-LEC Grown

Category Ceramic , Phosphide/Pnictide , Other Engineering Material , Semiconductor
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Gallium Phosphide Semiconductor Wafer, n-type, Sulfur + Tellurium Doped, Czochralski-LEC Grown.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of toward ; 3.5E+17 EDP/cm²; 5E+16-2E+17 CC-3
Physical Properties Metric English Comments
Density 4.13 g/cc
0.149 lb/in³