Material Notes:
Optical grade crystal with no small inclusions, cleavage planes, clouds and mist, point defects or bubbles inside the crystal. A proprietary process is used for cutting, grinding and polishing quality optical surfaces, producing high quality finished components that enable polarizers to be used with very high peak power lasers. Typical products are: rhombohedral shapes, rectangles and rounds, shaped plates, wedges, and cubes. Birefingent. Low susceptibility to moisture. Transparent 350 nm to 2300 nm.Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 2.71 g/cc
0.0979 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 3.1
3.1
Thermal Properties Metric English Comments
CTE, linear 5.68 µm/m-°C
3.16 µin/in-°F
ac
24.39 µm/m-°C
13.55 µin/in-°F
aa
Optical Properties Metric English Comments
Refractive Index 1.47744

@Wavelength 1.497 nm
1.47744

@Wavelength 1.497 nm
no
1.5114

@Wavelength 0.312 nm
1.5114

@Wavelength 0.312 nm
ne
1.63457

@Wavelength 1.497 nm
1.63457

@Wavelength 1.497 nm
no
1.71425

@Wavelength 0.312 nm
1.71425

@Wavelength 0.312 nm
ne
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
CaCO3 Content 99.94
Crystal Structure Crystalline Rhombohedral
Particle Shape Crystalline Rhombohedral