Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mapal Plastics Maplon Type S Polypropylene Sheet

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Mapal Plastics
Trade Name Maplon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mapal Plastics Maplon Type S Polypropylene Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
Thickness 1000 microns
39.4 mil
Surface Tension >= 48 dynes/cm
>= 48 dynes/cm
Up to 6 months
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 26.0 MPa

@Temperature 23.0 °C
3770 psi

@Temperature 73.4 °F
ASTM D638
Film Tensile Strength at Yield, TD 23.0 MPa

@Temperature 23.0 °C
3340 psi

@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, MD >= 650 %

@Temperature 23.0 °C
>= 650 %

@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, TD >= 300 %

@Temperature 23.0 °C
>= 300 %

@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, MD 23 %

@Temperature 23.0 °C
23 %

@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, TD 19 %

@Temperature 23.0 °C
19 %

@Temperature 73.4 °F
ASTM D638
Modulus of Elasticity 0.300 GPa

@Temperature 23.0 °C
43.5 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Izod Impact, Notched 1.00 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
1.87 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256
4.20 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.87 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy 5.50 J

@Temperature 23.0 °C
4.06 ft-lb

@Temperature 73.4 °F
ASTM D1709-85
Dart Drop Total Energy 55.0 J/cm

@Temperature 23.0 °C
0.103 ft-lb/mil

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Vicat Softening Point 140 °C
284 °F
ASTM D1525
Heat Distortion Temperature 80.0 °C
176 °F
ASTM D648
Descriptive Properties Value Comments
Color Mapal Color Catalogue No. 520002
Users viewing this material also viewed the following: